It looks like you are working on something interesting. I would guess 
that you are on to SMRF or some post yield issues.

The background report SAC95-09 shows on the table 4 on page 4-18:

A36

<Eagonzal(--nospam--at)ENG.CI.LA.CA.US> writes:
>Greetings:
>
>Does anyone know at what strain level does strain hardening occurs for 
>A36,
>A572, or rolled steel in general, and what is the approx. E after that 
>point
>but before Fu.?
>
>Thanks in advance
>ed gonzalez