In general, yes.

The CE is limited to 0.55 for A706 bar.  In general the CE's will be lower
and should be determined by the actual mill certs.  A CE of 0.45 is what is
considered weldable without preheat.  A CE of 0.55 can be welded with
preheat.  You would have to read the AWS for the particulars.