Unless you can
re-heattreat, I'd use O condition properties
Welds in 6061-T6 re age to a degree; use the Aluminum Association Structural Manual for guidance. Only the H- temper (work-hardened) alloys, commonly the 5000 series reverts to -O temper.
Christopher Wright P.E. |"They couldn't hit an elephant at
chrisw(--nospam--at)skypoint.com   | this distance" (last words of Gen.
.......................................| John Sedgwick, Spotsylvania 1864)
http://www.skypoint.com/~chrisw/


******* ****** ******* ******** ******* ******* ******* ***
*   Read list FAQ at: http://www.seaint.org/list_FAQ.asp
* * This email was sent to you via Structural Engineers * Association of Southern California (SEAOSC) server. To * subscribe (no fee) or UnSubscribe, please go to:
*
*   http://www.seaint.org/sealist1.asp
*
* Questions to seaint-ad(--nospam--at)seaint.org. Remember, any email you * send to the list is public domain and may be re-posted * without your permission. Make sure you visit our web * site at: http://www.seaint.org ******* ****** ****** ****** ******* ****** ****** ********